Several series of notch impact test samples were extracted transverse to the weld with notches positioned at the weld metal centre (WM), at the fusion line (FL), at the heat affected zone 2 mm from the fusion line (FL + 2 mm) and at 5 mm from the fusion line (FL + 5 mm).