First, the "empty POLICRYPS" structure has been infiltrated with the same curing mixture used for the fabrication of 1D POLICRYPS. A 2D grid
is then obtained by simply rotating the sample and following again the standard two-beam interference procedure utilized for the POLICRYPS fabrication, without the need of any multiple beam interference pattern.