As the specimen was gradually loaded (Fig. 8aed), isolated fractures
formed in various locations in the specimen (Fig. 8eeh). These fractures later coalesced to form more macroscopic fractures (Fig. 8iel). Fracturing of the triaxial specimen at s3 ¼1 MPa followed a similar trend as the uniaxial model.