Joint preparation shall be free from visible cracks. For steel grades higher than S460, cut areas shall be descaled by grinding, and verified to be free from cracks by visual inspection, dye penetrant or magnetic particle testing. Visible cracks shall be removed by grinding and the joint geometry corrected as necessary.