Specimen and experiment procedurSpecimen.The dimensions of the three-point bending specimen are 100mm in length, 2omm in width and 10mm in thickness. The length prior fatigue crack is made of 7075-T6 aluminum alloy and the common mechanical properties of the material are listed in Table1. e