Fig. 5 Fatigue crack propagation testing: crack growth rate(da/dN) versus stress intensity factor amplitude (DK) forbaseline epoxy and fullerene (C60) epoxy nanocomposites at*0.1, *0.5, and *1% weight of C60 nanoparticles. Insetshows the compact tension geometry used in the test